Product Process Main Uses Tensile strength (PSI)
CPCI 026 ARC Welding repair of foundry defects, also rectification of machining errors & buildup of worn out cast iron parts 60,000
Castron 223 ARC For heavy sections, maximum crack, resistance, machinable 57,000
Castron 224 ARC Thin sections, minimum dilution, outstanding machinability 50,000
Castron 242 ARC Minimum dilution grey cast iron, greater ease of application 50,000
Wunder 2240 ARC Penetrates contaminated cast iron surfaces, nodular deposits, machinable 58,000
Wunder 2233 ARC An innovative core wire design electrode for machinable welding of cast iron with maximum strength and crack resistance 72,000
Eutectrode 27 ARC Special designed non machinable cast iron electrode with strong arc force & clean action on contaminated cast irons