Description
Typical Charpy V-Notch Properties
| Impact Value | Testing Temperature | |||
| As Welded | ||||
| 35 J (26 ft-lb) | -196 degC (-321 degF) | |||
| 85 J (63 ft-lb) | -60 degC (-76 degF) | |||
| 110 J (81 ft-lb) | 20 degC (68 degF) | |||
Typical Tensile Properties
| Condition | Elongation | Tensile Strength | Yield Strength |
| As Welded | 30 % | 610 MPa (88 ksi) | 450 MPa (65 ksi) |
Recommended Welding Parameters
| Current | 150-260 A |
| Voltage | 24-29 V |
| Wire Diameter | 0.047 in. |
| Wire Diameter | 1.2 mm |
| Wire Feed Speed | 118-394 in./min |
| Wire Feed Speed | 3.0-10.0 m/min |
Classifications
| Wire Electrode | EN ISO 14343-A : G 23 12 L SFA/AWS A5.9 : ER309L |
Approvals
| Approvals | CE EN 13479 VdTÜV 02103 |
| Approvals are based on factory location. Please contact ESAB for more information. |
Consumable Characteristics
| Alloy Type | Austenitic (with approx. 14 % ferrite) 24 % Cr – 13 % Ni – Low C |
Typical Weld Metal Analysis %
| Typical Wire Composition % | ||||||||||||||
| C | Co | Cr | Cu | Mn | Mo | N | Ni | P | S | Si | ||||
| <=0.015 % | <=0.05 % | 24 % | <=0.10 % | 1.8 % | <=0.3 % | <0.06 % | 13 % | <=0.015 % | <=0.015 % | 0.3 % | ||||