EXATON 317/317L

317/317L is suitable for joining stainless CrNiMo steels e.g. 317L or similar. It is used for MIG/MAG welding.

Category:

Description

Typical Charpy V-Notch Properties

As Welded
Impact Value 104 ft-lb
Impact Value 140 J
Testing Temperature 68 °F
Testing Temperature 20 °C

Typical Tensile Properties

Condition Elongation Tensile Strength Yield Strength
As Welded 42 % 600 MPa (87 ksi) 380 MPa (55 ksi)

Recommended Welding Parameters

Current 150-260 A
Voltage 24-29 V
Wire Diameter 0.047 in.
Wire Diameter 1.2 mm
Wire Feed Speed 118-394 in./min
Wire Feed Speed 3.0-10.0 m/min

Classifications

Wire Electrode SFA/AWS A5.9 : ER317L
Werkstoffnummer : 1.4438*
EN ISO 14343-A : G 19 13 4 L

Typical Weld Metal Analysis %

Typical Wire Composition %
C Cr Cu Mn Mo Ni P S Si
<=0.02 % 19 % <=0.3 % 1.5 % 3.6 % 14 % <=0.020 % <=0.020 % 0.4 %